2026 Catalog - Flipbook - Page 19
Web Slings
Shortening of the sling length.
Lift-All nylon and polyester web slings shall be
permanently removed from service when the cumulative
UV or outdoor exposure has reached these limits:
•
•
Reduction in elasticity of the sling.
Breakage or damage to yarn 昀椀bers is often
evident by a fuzzy appearance on the web.
•
Sti昀昀ening of the web.
1-Ply and 2-Ply web slings
3 years:
3-Ply and 4-Ply web slings
Temperature
Nylon and polyester slings degrade at temperatures
above 200°F.
Chemical Environment Data
Lift-All webbing is treated for abrasion. Heavy
duty treatments are available as a supplemental
process for greater protection. Natural, untreated
webbing is available upon request.
Many chemicals have an adverse e昀昀ect on nylon and
polyester. The chemical chart below is a general guide
only. For speci昀椀c temperature, concentration and time
factors, please consult Lift-All prior to purchasing or use.
NYLON
POLYESTER
10%
Treated
7%
Natural
6%
Natural
3%
Length Tolerance*
1-Ply
± (1.5" + 1.5% of sling length)
2-Ply
± (2.0" + 2% of sling length)
3-Ply & 4-Ply
± (3.0" + 3% of sling length)
+
NO
OK
OK
OK
NO
OK
OK
OK
OK
OK
OK
OK
OK
OK
OK
OK+
OK
NO
NO
OK
OK
OK
OK
OK
OK
OK
OK
OK
OK
OK
Disintegrated by concentrated sulfuric acid.
Lifting
Devices
* For web sling widths wider than 6", add 1/2" to these values.
For tighter tolerance or matched set lengths, please consult
with Customer Service prior to ordering.
Acids
Alcohols
Aldehydes
Alkalis
Bleaching Agents
Dry Cleaning Solvents
Ethers
Halogenated Hydro-Carbons
Hydro-Carbons
Ketones
Oils Crude
Oils Lubricating
Soap & Detergents
Water & Seawater
Weak Alkalis
Plate
Clamps
Sling Type
POLYESTER
Hoist
Rings
TOLERANCES FOR WEB SLINGS
NYLON
Lift-All
Hoists
Treated
CHEMICAL
Cargo
Control
The stretch characteristics of web slings depends
on the type of yarn and the web treatment.
Approximate stretch at rated sling capacity:
Mesh
Slings
Elasticity
Rigging
Hardware
Anti-Abrasion Treatment
Chain
Slings
•
2 years:
Wire
Rope
Accelerated abrasive damage to the surface
yarns of the sling.
Sling
Protection
•
•
•
Uneven or disoriented surface yarn of the
webbing.
Round
Slings
Fading of webbing color.
Nylon and polyester web slings possess a limited useful
service life due to the degradation caused by exposure
to sunlight or other measurable sources of UV radiation.
Lift-All web slings that are regularly exposed to UV
radiation should be identi昀椀ed with the date they are
placed into service and should be proof-tested to twice
their rated capacity every six months.
Visible indication of such environmental
deterioration can include the following:
•
•
Sunlight / UV Exposure Service Life
Web
Slings
Exposure to sunlight and other environmental
factors can result in accelerated deterioration of
web slings. The rate of this deterioration varies
with the level of exposure and with the thickness of
the sling material.
General
Information
ENVIRONMENTAL CONSIDERATIONS
Prior to sling selection and use, review and understand the General Information section of this catalog.
17